I'm really keen to start refining copper & silver using a plating bath & a generator powered by a small windmill.
8 Foot high or such.
I have about 50Kg of black & green solid that I have washed off burnt copper wire, planning on converting it back to copper & then maybe looking into the silver side of things.
I did make a tiny electroplating plant from a 'solar powered garden light' I found.
It did what I thought it would. Plated solidly. A 7/8th square copper ingot.
Then when I went to using a transformer, it blew out, dunno about using it 24hrs a day, hence the windmill.
Any suggestions? I think the Anode should be Titanium, or under the copper oxide in the bottom of the tub.
Maybe a stirrer in there as well?