Originally Posted by
cyberdan
It is still my TV days. out of all my CRT's I have only gotten one AL degaussing cable. Now I always cut before removing the sticky cover.
Last month I was stripping a motor and cut off one end of the stator. I saw white metal so threw in scrap pile. After I took it in and gave to owner I noticed only half the windings were AL the rest was CU. Too late he already had it. I now check everything.
Agree, the same with transformers. I've been cutting mine for the last 2 weeks? I found 2 that were aluminum and maybe 6 that were aluminum on the outside and copper on the inside.