Results 1 to 20 of 22

Di cast Zink or Lead

| A Day in the Life of a Scrapper

Hybrid View

  1. #1
    BarrenRealms007's Avatar
    SMF Badges of Honor

    Member since
    Jun 2012
    Location
    Arkansas
    Posts
    397
    Thanks
    180
    Thanked 325 Times in 147 Posts
    If you want to test it put a small amount in some Hydrochloric acid. Zinc will react and dissolve in the solution lead will not. Aluminum will also react with the solution.

    We buy electronic scrap, Gold Karat scrap, gold filled, refined gold, silver and many other item's.

  2. The Following 2 Users say Thank You for This Post by BarrenRealms007:


  3. #2
    Copper Head is offline Metal Recycling Entrepreneur
    Copper Head started this thread.
    Copper Head's Avatar
    SMF Badges of Honor



    Member since
    Aug 2011
    Location
    Up North
    Posts
    1,883
    Thanks
    579
    Thanked 1,014 Times in 516 Posts
    Quote Originally Posted by BarrenRealms007 View Post
    If you want to test it put a small amount in some Hydrochloric acid. Zinc will react and dissolve in the solution lead will not. Aluminum will also react with the solution.
    I can get my hands on muriatic acid , If I mix salt with muriatic will it be like a weak version Hydrochloric acid.
    muriatic acid, and spirits of salt = Hydrochloric acid.
    Bottom line using any acid I guess lead will not be reactive
    so next question : is Zinc more reactive then AL ? (faster to dissolve)

  4. #3
    BarrenRealms007's Avatar
    SMF Badges of Honor

    Member since
    Jun 2012
    Location
    Arkansas
    Posts
    397
    Thanks
    180
    Thanked 325 Times in 147 Posts
    Quote Originally Posted by Copper Head View Post
    I can get my hands on muriatic acid , If I mix salt with muriatic will it be like a weak version Hydrochloric acid.
    muriatic acid, and spirits of salt = Hydrochloric acid.
    Bottom line using any acid I guess lead will not be reactive
    so next question : is Zinc more reactive then AL ? (faster to dissolve)
    Hydrochloric and Muriatic Acid are the same thing just some times in different strenghts but usuasly and the most concentrated is 32%.

    Aluminum is more reactive than zinc, especialy if the solution is heated you can count on a boil over from your reaction vessel with aluminum because of the volume increase from the reaction.

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

 
Browse the Most Recent Threads
On SMF In THIS CATEGORY.





OR

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  

The Scrap Metal Forum

    The Scrap Metal Forum is the #1 scrap metal recycling community in the world. Here we talk about the scrap metal business, making money, where we connect with other scrappers, scrap yards and more.

SMF on Facebook and Twitter

Twitter Facebook